Oh, I’m a-doin’ it.

This part is actually slightly outside the “safe print zone” dashed lines on my build plate. I put down like half a can of hairspray on it right before the nozzle descended. Wish me luck.

  • jokeyrhyme@lemmy.ml
    link
    fedilink
    English
    arrow-up
    2
    ·
    4 hours ago

    huh, hair spray, makes sense

    i’ve been using an FDM-specific spray, but I bet hair spray is more cost effective

    • dual_sport_dork 🐧🗡️@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      1
      ·
      3 hours ago

      There are some materials where that’s probably a better idea. Polycarb or Nylon leap to mind. But for PLA, PETG, ABS/ASA, etc. I’ve found that hairspray works just fine. I’ve been doing it for years.